FPM 80 Nr. : FP 80 01 30
Colour : black
Properties | Testing Method | Testing Parameter | Value | Units |
Hardness | ASTM D 2240 | - | 80 ± 5 | Shore A |
Tensile strength | ASTM D 412 C | - | 14 | N/mm2 |
Ultimate elongation | ASTM D 412 C | - | 170 | % |
Low temp. resistance | ASTM D 1329 ASTM D 746 |
TR10 2 min / -22 °C |
-17 pass |
°C - |
Compression set | ASTM D 395 B | 70 h / 200 °C | 20 | % |
Changes of properties after ageing acc. to ASTM D 471 / 573 in:
Test Parameter Medium |
Volume % | Hardness | Tensile Strength % | Ultimate Elongation % |
Luft / Air 70 h / 250 °C |
- | +2 | -4 | +8 |
ASTM Fuel C 70 h / 23 °C |
+4 | -4 | -16 | -17 |
ASTM Oil No.3 70 h / 150 °C |
+2 | -1 | -10 | -9 |
Compliant with the EU-directives 2000 / 53 / EG (ELV), 2002 / 95 / EG (RoHS) and 2006 / 122 / EG (PFOS).
The results displayed in this data sheet were obtained on standard test specimens following standard test procedures. Comparisons with
results obtained on finished products, e.g. O-Rings, could lead to other results due to differences in geometry and manufacturing processes.
These other results do therefore not automatically contravene the data of this sheet. The evaluation of parts prior to their use in order to
ensure their suitability for the intended application is subject to the end user's responsibility.